KTP - KTiOPO4
Parameters
- Phase Match Type II
- Non-Linear Coeffecient 3.18 x10^-12 m/V at 1064nm to 532nm
- Refractive Index 1.74
- Absorption .010 cm^-1
- Transparent Range 350nm to 4000nm
- Required Power Density 200MW/cm^2
- Damage Threshold 500MW/cm2
- Phase Matching Angle 24.3 deg
- Walk-off Angle .26 Deg
- Melting Point 1150 deg C
- Lifetime at 80 Deg C and 150MW/cm^2 20 x 10^7 pulses
Tolerance Parameters (FWHW)
- Angular 25 mr-cm
- Thermal 25 Deg C-cm
- Spectral .56 nm-cm